Austenitic stainless steel castings
CF8M Cast Stainless Steel
CF8M is a casting designation. Specify the casting standard and revision rather than ordering it solely by a related wrought-steel name.
Identity and reference basis
CF8M is a casting designation. Specify the casting standard and revision rather than ordering it solely by a related wrought-steel name.
Search names: CF8M; J92900; 316 comparison only; 铸造不锈钢
Search names identify this record; they are not an approval to substitute grades or supplier formulations. Specify the exact ordered material and product standard.
Technical reference parameters
| Parameter | Reference value | Basis and conditions |
|---|---|---|
| Carbon | ≤0.08 wt.% | Historical summary reference. |
| Chromium / nickel | 18.0–21.0 / 9.0–12.0 wt.% | Historical summary ranges. |
| Molybdenum | 2.0–3.0 wt.% | Historical summary limit/range. |
| Tensile strength | ≥485 MPa | Solution-treated reference in the cited summary. |
| 0.2% offset yield strength | ≥205 MPa | Same historical summary basis. |
What to confirm for a component
- Casting standard and revision, grade and heat treatment.
- Drawing, casting route, machining allowances and traceability.
- Agreed inspection, repair-welding and acceptance criteria.
Provide the drawing, intended service conditions, quantity and acceptance requirements. Agree the delivered specification before using a reference value in component design.
Source and data conditions
SFSA Steel Castings Handbook Supplement 2 (2017): ASTM A351/A351M-16 summary
Manufacturer or technical-association reference, reviewed 25 November 2026. Named commercial grades identify the cited example; no manufacturer affiliation, approval or stock availability is implied. Values are references for the stated material and conditions, not AODSON batch test results.
Product form, joining and manufacturing review
The associated wrought comparison (316) is a search aid, not an approved substitute. On an RFQ, specify casting geometry, section transitions, machined sealing surfaces and inspection access. Agree any repair-welding procedure, subsequent heat treatment and final inspection before production. Verify chemistry, test-coupon requirements and certificates against the ordered casting specification; do not import bar or tube properties into the casting.
Explore related records and compare their stated conditions.
Compare casting grades
Selection for a finished component
Questions that determine suitability
For a proposed CF8M housing, fitting or bracket, identify the working medium, cleaning chemicals, temperature and crevice geometry. Review the casting specification and final treatment together with the component drawing.
Before approving a substitution
If welding or repair welding is part of production, review the ordered carbon limits and final treatment rather than assuming a general stainless designation settles weld acceptance. The molybdenum-bearing grade is not a universal approval for seawater or any chloride concentration.
Manufacturing and acceptance review
Mark pressure boundaries, seal faces, thread locations and visible surfaces before planning casting allowance and finish machining. Specify examination coverage, acceptance criteria and leak testing separately where required; identify which tests apply after any approved repair.
These component-review questions complement the cited material reference; they do not add guaranteed properties or certify a manufacturing route.
Continue the material review.
Return to the library to compare records, or discuss the material requirement for your component.